Diamond TMT 500+D

Fe-500+ D

Diamond TMT 500+ D

Chemical Properties

Carbon

0.250


Sulphur

0.035

Phosphorus

0.035


S & P

0.070

Mechanical Properties

Yield stress

520 min

Tensile strength

600


Elongation

18 min

With Standard Bars

Comparision

 
  Chemical Properties
# Bars Carbon(%) Sulphur(%) Phosphorus(%) S & P(%)
1 IS 1786:2008 0.250 0.040 0.040 0.080
2 Diamond TMT Fe-500 0.250 0.035 0.035 0.070
*Lower Sulphur and Phosphoros Properties compared to the IS 1786 Standard reveal our product is more durable than the Standards Specified